| Contact Us   Global
AFM Probe Selection Guide
How to choose an AFM probe
AFM Probe Selection Guide Book
DOWNLOAD

SSRM

For optimal performance with our AFM systems please request a quote from Park Systems. Mounted cantilevers are additionally tested. All probes that are not listed here from Adama Innovations, Applied Nano Structures, Inc, BudgetSensors, MikroMasch, Nanosensors™, Nanotools GmbH, Nanoworld AG, NuNano, Olympus Corp., are possible to order from our probe store. Probes from other manufacturers also can be possible to order upon request for quotation. The performance of probes ordered from other sources are not guaranteed.

Probe Force Constant (N/m) Frequency (kHz ) Manufacture Short Description Quote
CDT-NCHR 80 400 Nanosensors ▪ Cantilever suitable for SSRM/lithography
▪ Backside reflex coating (Al)
▪ Electrically conductive diamond-coated tip
▪ Mounted type on Conductive AFM (C-AFM) Chip Carrier
Request for Quote
Property Nominal Value Specified Range
Thickness /µm 4 3.0 - 5.0
Mean Width /µm 30 22.5 - 37.5
Length /µm 125 115 - 135
Force Constant /(N/m) 80 23 - 225
Resonance Frequency /kHz 400 225 - 610
CAMS FDP 27
11
3
  imec ▪ Full diamond probes for SSRM
▪ Solid boron-doped polycrystalline diamond tip
▪ 3 cantilevers with different spring constants on a chip
▪ Mounted type on Conductive AFM (C-AFM) Chip Carrier
Request for Quote
Cantilevers Spring Constant
(N/m)
Length
(µm)
Width
(µm)
Thickness
(µm)
nominal range nominal nominal ±1
Short 27 14-47 225 50 5
Medium 11 5-19 305 50 5
Long 3 1-6 465 50 5

Experience our product's high-quality, precise, and long life backed by our worldwide service network. We are strongly committed to maintaining the quality of our products, making us a trustworthy choice for all your repair and maintenance needs.

We await your inquiry and will arrange for you to speak with a specialist today to explore tailored solutions for your research needs. Please fill out the form now, and we will promptly get in touch with you.

Don't miss out on new product announcements, the latest tech insights, special events, and more. Subscribe now to receive regular updates straight to your inbox!