block_copolymer GlassTemperature MechanicalProperty KAIST CeramicCapacitor Metal YttriaStabilizedZirconia FrictionalForceMicroscopy P3HT China PolymerBlend LiIonBattery EvatecAG contact ito_film IVSpectroscopy Wildtype Chungnam_National_University exfoliate CaMnO3 LateralForce Celebration SingleLayer Piranha TappingMode Edwin Morphology MonoLayer Litho LiBattery HighAcpectRatio Barium_titanate KelvinProbeForceMicroscopy polymeric_arrays temp_control
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Atomic steps on GaP(Gallium Phosphide) layer on Si
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: PPP-NCHR (k=42N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 512×512