Cobalt-dopedIronOxide Spain Phenanthrene Vacuum Formamidinium_lead_iodide ULCA ferromagnetic ThermalConductivity Christmas BTO Sadowski IndiumTinOxide Pyroelectric Ceramic PvdfBead GaAs MESA structure CrossSection Current HexagonalBoronNitride Adhesive Array StyreneBeads MolecularSelfAssembly University_of_Regensburg HiVacuum Zhi Implant ItoGlass ito_film KevlarFiber Materials amplitude_modulation fluoroaalkane SiliconOxide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PMN-PT single crystal
Scanning Conditions
- System: NX10
- Scan Mode: PFM
- Cantilever: NSC36A Ti-Pt (k=1N/m, f=90kHz)
- Scan Size: 8μm×8μm
- Scan Rate: 0.5Hz
- Pixel: 512×256