H-BN HexagonalBN LiNbO3 Electrical&Electronics HafniumDioxide Blood pulsed_laser_deposition SurfaceOxidation aluminum_nitride Etch Copper Ferrite NiFe MagneticPhase amplitude_modulation thermal_property OrganicSemiconductor heterojunctions hard_disk AM-KPFM high_resolution OpticalWaveguides Fiber atomic_steps mechanical property MoirePattern Hexatriacontane 2d_materials semifluorinated alkane optoelectronics MfmPhase semifluorinated_alkanes WPlug EFM plastics
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe-Nd-B
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact, TCS
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×256
- TCS: Temperature control stage type2