Cell tip_bias_mode ScanningThermalMicroscopy Graphene frequency_modulation Terrace ThermalDetectors InsulatorFilm MfmAmplitude GalliumPhosphide Yeditepe_University AnodizedAluminumOxide Inorganic_Compound Granada TemperatureControl Temasek_Lab Change OpticalWaveguides SolarCell AtomicLayer Calcium LiquidCrystal Bio Mechanical&nanotechnology DeflectionOptics NanoLithography HfO2 HiVacuum mechanical property C60H122 ContactModeDot Pzt AIN LightEmission Graphite
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Lithography on Si substrate
Scanning Conditions
- System: NX10
- Scan Mode: Lithography
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel: 1024×512
- Litho. mode: Tip bias mode
- Litho. Tip bias: Black -10V, White 0V