TriGlycineSulphate Terrace flakes Litho Change PVAP3HT GranadaUniv VerticalPFM Formamidinium_lead_iodide aluminum_nitride Gold ferromagnetic Vinylpyridine MembraneFilter ULCA vertical_PFM Wonseok IRDetector Conductance suspended_graphene TungstenThinFilmDeposition Memory GlassTemp Fujian Magnetic Force Microscopy PinPointMode NeodymiumMagnets Morphology Ca10(PO4)6(OH)2 Aggregated_molecules OpticalWaveguides Lattice Sperm GaAs Stiffness
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BTO
Scanning Conditions
- System: XE7
- Scan Mode: DC-EFM(Vertical)
- Cantilever: ElectriMulti75G (k=3N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.2Hz
- Pixel: 256×256
- Sample Bias: 0V
- Tip Bias: 1V ac
- Scan Mode: DC-EFM(Vertical)
- Cantilever: ElectriMulti75G (k=3N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.2Hz
- Pixel: 256×256
- Sample Bias: 0V
- Tip Bias: 1V ac