CBD Mechanical self_assembly CopperFoil frequency_modulation GlassTemperature Collagen Yttria_stabilized_Zirconia MBE Mobile HydroGel NCM\ Mechanical&nanotechnology Led HighAcpectRatio Polymer OrganicCompound Fiber CeNSE_IISc TemperatureControl hard_disk Polyethylene NtuEee Magnetostrictive light_emission layers OpticalElement FM-KPFM BoronNitride CancerCell Forevision DiffractiveOpticalElements AM_KPFM Nanotechnology Jason
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Collagen film phase change by temp
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan