LaAlO3 HDD HexagonalBoronNitride FM_SKPM Blend Vac Chemical_Vapor_Deposition Boron block_copolymer FloppyDisk INSP Led organic_polymer PatternedSapphireSubstrat ForceVolumeImage Oxide silicon_oxide TappingMode cannabidiol MultiferroicMaterials Polyvinylidene Titanate Nanofiber Switching Dr.JurekSadowski ElectroDeposition Fendb KAIST Ni81Fe19 VerticalPFM LeakageCurrent BFO SiliconCrystal Ptfe SRAM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256