Composite Barium Titanate

Composite Barium Titanate

PFM Quad color is overlaid on 3D surface morphology.

Scanning Conditions

- System: NX10
- Scan Mode: PFM
- Cantilever: PPP-ContScPt (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 256 × 256