TCS DOE Iron Optical PVA Self-assembledMonolayer ConductiveAFM cannabinoid Flake BTO Multiferroic_materials Inorganic Pyroelectric KAIST Electrical&Electronics PANI cannabis Water Trench Electronics MechanicalProperty strontiu_titanate Solar thermal_property Zhi high_resolution hetero_structure LifeScience Polyurethane Moire C_AFM HardDiskMedia Korea FrictionalForce Spain
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256