Zhi FrictionalForceMicroscopy TemperatureControl ConductiveAFM VortexCore DataStorage GlassTemp 2d_materials NUS WWafer thermal_conductivity HiVacuum ElectrostaticForceMicroscopy Hexacontane EFMAmplitude LiquidCell Gallium_Arsenide Composition fluoroaalkane pinpoint mode Tungsten_disulfide AdhesionEnergy tip_bias_mode HumanHair Current Hexylthiophene doped Nanotechnology Sidewall cannabinoid DLaTGS KAIST Ceramics Pattern ThermalConductivity
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256