OrganicCompound Defects Conductivity light_emitting LiquidCell Barium_titanate Techcomp Defect BreastCancerCell Zhi Polyimide Ceramic Christmas India F14H20 Polyvinylidene_fluoride exfoliate Spincast Ito HardDisk temperature controller AFM MoS2 Conducting Ecoli UTEM BismuthVanadate NanoLithography lift_mode SFAs Electical&Electronics FAFailureAnlaysis PetruPoni Growing Cobalt-dopedIronOxide fluoroaalkane
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Margarines
Phase change of Margarine surface by temperature control
Scanning Conditions
- System: NX10
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256