align Aluminium_Oxide Polystyrene fluoroaalkane SmallScan Cobalt-dopedIronOxide Graphene Boundary high_resolution Biofilm SrTiO3 PvdfFilm Electrode ForceMapping Flake Protein HOPG Hair BloodCell CancerCell Sio2 Current Permalloy University_of_Regensburg Leakage AM-KPFM BaTiO3 Granada CrystalGrowing BariumTitanate cannabinoid Blend TungstenDeposition multi_layer Metal
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Copper Foil
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.5Hz
- Pixel: 512512