MoS2 (1/2)

MoS2 122 2

Scanning Conditions

- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 30μm×30μm
- Scan Rate: 0.1Hz
- Pixel: 512×1024