Optical Hexylthiophene IVSpectroscopy electrospinning Gallium_Arsenide MoirePattern LiquidImaging Dopped ForceVolumeImage margarine Anneal Christmas PetruPoni Chemical_Vapor_Deposition MLCC Galfenol CalciumHydroxyapatite Bacteria PpLdpe Leakage Water graphene_hybrid doped NusEce Piezoresponse GaN NUS_NNI_Nanocore Electronics dichalcogenide Composite HydroGel DLaTGS TungstenThinFilmDeposition Molybdenum block_copolymer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36C Cr-Au(k=0.6N/m, f=65kHz)
- Scan Size: 12μm×12μm
- Scan Rate: 0.15Hz
- Pixel:256×256
- Scan Mode: KPFM
- Cantilever: NSC36C Cr-Au(k=0.6N/m, f=65kHz)
- Scan Size: 12μm×12μm
- Scan Rate: 0.15Hz
- Pixel:256×256