ImideMonomer self_assembly Mechanical&nanotechnology LateralPFM contact Yttria_stabilized_Zirconia Hexatriacontane OpticalModulator CancerCell Pzt Cobalt C36H74 Phthalocyanine Magnetostrictive temp Boundary Pipette Pvdf Bacteria Heating mechanical_property Calcite Bmp Fe_film organic_polymer DiffractiveOpticalElements Battery plastics Sphere STO Nanofiber Temperature cannabinoid FAFailureAnlaysis Flake
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Patterned Sapphire Substrate (PSS)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR
- Scan Size: 40μm×40μm, 3μm×3μm
- Scan Rate: 0.3Hz, 1Hz
- Pixel: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR
- Scan Size: 40μm×40μm, 3μm×3μm
- Scan Rate: 0.3Hz, 1Hz
- Pixel: 256 × 256