Scanning_Thermal_Microscopy HOPG Wildtype Hafnia FM_SKPM bias_mode Tapping LiNbO3 Pyroelectric Regensburg Resistance NeodymiumMagnets Cobalt-dopedIronOxide MfmPhase fluoroaalkane Chungnam_National_University Silicon Display MLCC MultiferroicMaterials ElectroChemical TyphimuriumBiofilm Annealed Scratch Nanotechnology Titanate NCM\ SrTiO3 Calcium dielectric trench Global_Comm MultiLayerCeramicCapacitor EFMAmplitude PhaseTransition Vinylpyridine
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256