AtomicLayer NUSNNI thermal_property Polystyrene LightEmiting TemperatureControl Christmas AM_SKPM NUS_NNI_Nanocore Polyurethane DOE molecular_beam ThermalConductivity AnodizedAluminumOxide nanomechanical Morphology Vortex self_assembly SThM Conductance Crystal SiliconCrystal AlkaneFilm Fet Varistor FuelCell C36H74 ItoGlass DiffractiveOpticalElements Fendb BloodCell Hexatriacontane Boron PhthalocyaninePraseodymium Molybdenum
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Atomic steps on STO(110)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: PPP-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.62Hz
- Pixel: 512×512