Electrode FAFailureAnlaysis TungstenThinFilmDeposition BiasMode self-assembly Dopped aluminum_nitride MoS2 semifluorinated alkane piezoelectric force microscopy Typhimurium StainlessSteel Biology flakes Inorganic Etch LithiumNiobate KAIST cooling IndiumTinOxide hetero_structure PolycrystallineFerroelectricBCZT Laser ElectrostaticForceMicroscopy SRAM SolarCell Yeditepe mechanical property SingleLayer IVSpectroscopy NUS_Physics Floppy temperature_control PolymerPatterns HiVacuum
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
P(VDF-TrFE-CFE)
Scanning Conditions
- System : FX40
- Scan Mode: Tapping
- Scan Rate : 0.5 Hz
- Scan Size : 2μm×2μm
- Pixel Size : 512×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)