Tape alkanes 2-vinylpyridine HexagonalBoronNitride LowDensityPolyethylene fluoroalkane temperature_control SmallScan MBE Electical&Electronics Bacteria Phenanthrene cannabinoid Floppy Fujian MagneticPhase I-VSpectroscopy Piezoelectric Jason MagneticForce Celebration PVAP3HT ConductiveAFM FAPbI3 AM_SKPM StainlessSteel Polystyrene AdhesionForce SiliconOxide Iron semifluorinated alkane YttriaStabilizedZirconia MolybdenumDisulfide Aggregated_molecules CaMnO3
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Plate-shaped DNA origami
Scanning Conditions
- System : FX40
- Scan Mode: Tapping in Liquid
- Scan Rate : 1Hz
- Scan Size : 250nm×250nm
- Pixel Size : 512×256
- Cantilever : USC-F0.3-k0.3 (k=0.3N/m, f=300kHz)