VortexCore Adhesion semifluorinated alkane Ferroelectric PVAC HiVacuum fluoroalkane PolyvinylideneFluoride Bismuth Molybdenum_disulfide OxideLayer Graphite Electrical&Electronics Piranha Chemical Vapor Deposition NUS_Physics Spincast PetruPoni_Institute PolyStylene SingleCrystal Logo LaAlO3 Chloroform sputter StrontiuTitanate self-assembled_monolayer PS_LDPE LateralPFM StyreneBeads Display MolybdenumDisulfide OpticalWaveguide PolyvinylAcetate Gong Copper
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferroelectric 2L-hBN
Scanning Conditions
- System : FX40
- Sample bias: 0.25 V, 0.8 V
- Scan Mode: C-AFM
- Scan Rate : 8 Hz
- Scan Size : 1.5μm×1.5μm
- Pixel Size : 256×256
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)