NUSNNI GalliumPhosphide ito_film Corrosion mechanical property Vortex Polyvinylidene_fluoride align MagneticPhase LiIonBattery PhthalocyaninePraseodymium AM_KPFM DLaTGS optoelectronics TemperatureControllerStage Titanate SiliconeOxide AtomicLayer AIN PFM F14H20 Piezoelectric Temasek_Lab SiliconOxide BCZT OpticalWaveguides Varistor Moire Styrene HanyangUniv Polydimethylsiloxane ConductiveAFM rubber NCM\ EFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hair
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel: 512×256