tip_bias_mode #EC Sidewall biocompatible strontiu_titanate ShenYang Phosphide PVA Conductive AFM TempControl temp_control MultiLayerCeramicCapacitor PMNPT ConductingPolymer Spincast non_contact Optic InorganicCompound PtfeFilter polyvinyl acetate electrospinning Laser self_assembly FastScan SmallScan ImideMonomer Conductivity Jason MoirePattern mono_layer Copolymer temp LiquidImaging LFM AnodizedAluminumOxide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PZT thin film
Scanning Conditions
- System: NX10
- Scan Mode: PFM (DC-EFM)
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512