Piranha LaAlO3 Bismuth PolymerPatterns Modulus Ceramic Growing VortexCore gallium_nitride Chungnam_National_University organic_polymer Non-ContactMode Logo Collagen Glass PVAP3HT Tungsten NeodymiumMagnets Fet Styrene Gallium_Arsenide lift_mode IndiumTinOxide Self-assembledMonolayer Battery C36H74 MBE FloppyDisk MechanicalProperty NusEce Steps Mechanical&nanotechnology Zagreb Gold Pinpoint PFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG Moire
Scanning Conditions
- System: NX10
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128