DiffractiveOpticalElements Battery mechanical property Ananth Barium_titanate DentalProsthesis self_healing hard_disk_media CrAu BFO dichalcogenide Roughness Worcester_Polytechnic_Institute Pore Titanate Polytetrafluoroethylene Genetic self-assembly Ni-FeAlloy ThermalProperties MetalCompound ChemicalCompound Hexatriacontane NUSNNI PhaseImaging SKPM electrospinning CompactDisk Chungnam_National_University CopperFoil Hair lift_mode Solar domain_switching Beads
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic Vortex Core (Ni-Fe alloy)
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: LM-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.2Hz
- Pixel: 1024×1024
- Lift Height: 80nm
- Scan Mode: MFM
- Cantilever: LM-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.2Hz
- Pixel: 1024×1024
- Lift Height: 80nm