Platinum conductive hard_disk_media FailureAnlaysis IISCBangalore INSPParis exfoliate Gold ScanningIon-ConductanceMicroscopy graphene_hybrid Piezoelectric BreastCancerCell PolyvinylAcetate IVSpectroscopy Lift fluorocarbon Austenite CuSubstrate OrganicSemiconductor Oxidation silicon_carbide Chromium Modulus Magnets HydroGel hard_disk C_AFM Polyimide nanobar Co/Cr/Pt semifluorinated alkane SSRM Logo CaMnO3 AtomicSteps
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CrAu surface
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 256×256