SICM MoirePattern Friction LifeScience AAO PS_PVAC Reduction Ito HydroGel LaAlO3 Worcester_Polytechnic_Institute ForceVolumeMapping GalliumPhosphide Hafnium_dioxide SRAM Vacuum Chloroform PVAP3HT Croatia light_emitting Sphere biocompatible Insulator TransitionMetal Conductive AFM bias_mode ScanningTunnelingMicroscopy Composition FrequencyModulation Spincast Memory chemical_compound Polyaniline OrganicCompound Pyroelectric
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PDMS liquid crystal
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×512