SPM Study of Tribo-Photovaltaic Effect in Metal, Semiconductor Moving Contacts

Speaker : Jun Liu Affiliation : University at Buffalo Region : US Year : 2019 Language : English Explore the groundbreaking discovery of the Tribo-Photovoltaic Effect in Metal-Semiconductor Moving Contacts through SPM study. Uncover the unique interplay of mechanical and electrical forces, potentially revolutionizing energy harvesting and sensing applications.