Electrical and Surface Characterization of Ga-Assisted MBE Grown Be-Doped GaAs Nanowires and Te-Doped GaAsSb Nanowires for Infrared Photodetector Application
Speaker : Priyanka Ramaswamy Affiliation : Department of Electrical and Computer Engineering, North Carolina A&T State University, Greensboro Region : LatAm Year : 2021 Language : English Explore the assessment of dopants in semiconductor nanowires using advanced characterization techniques. Discover insights into carrier concentration modulation and material properties without contact fabrication, crucial for optoelectronic device engineering.