Piezoelectric and electrostatic properties of electrospun PVDF-TrFE
nanofibers and their role in electromechanical transduction in nanogenerators and strain sensors
Speaker : Ass. Prof. Tobias Cramer Affiliation : University of Bologna, Italy Region : Europe Year : 2020 Language : English Explore the fabrication and characterization of PVDF-TrFE nanofibers for flexible electronic transducers. Learn about their piezoelectric and electrostatic properties, and their role in electromechanical transduction for nanogenerators and strain sensors.