Electrochemical AFM (EC-AFM): Copper Deposition/ Dissolution on Gold - August 11, 2020
SPEAKERS
-
Jiali Zhang
Park Systems Inc., Santa Clara, California, USA
- Jiali Zhang, Ph.D., is an engineer for Park Systems, where she focuses on the installation and support of AFM systems for Park’s research user base. She is also responsible for researching and writing technical papers and application notes for publication and presentation at scientific conferences. She received her Ph.D. in Analytical Chemistry from the University of California, Davis, and holds a B.S. in Applied Chemistry from Donghua University in Shanghai, China. Her expertise spans numerous microscopy techniques, and areas of study have also included biological systems and 3D printing technologies.
- Access Speaker Publications
SPEAKERS
-
- Jiali Zhang
- Park Systems Inc., Santa Clara, California, USA
Authors
The applications team at Park Systems is proud to present an introduction to electrochemical atomic force microscopy (EC-AFM), a characterization technique derived from Atomic Force Microscopy (AFM) that can be used for monitoring the electrodeposition process during electrochemical reactions. The cyclic voltammetry (CV) technique is typically employed to investigate the electrochemical reaction mechanisms using an electrochemistry cell and a choice of potentiostat or galvanostat.
This webinar explains the basics of EC-AFM and investigation of localized electrochemical deposition and dissolution of copper using the Park NX12 AFM System.
Related Contents
System Webinars
What can we learn from scanning electrochemical probe microscopy (SEPM) studies on interfaces and interphases of battery electrodes
System Webinars
From Single Hologram to 3D Volumetric & 4D Time-Resolved Insight in Various Fields of Science
System Webinars
Beyond Conventional Ellipsometry: High-Resolution Mapping of Oxide Thin Film
×