Film Polydimethylsiloxane Mosfet Tungsten_disulfide Pinpoint PFM silicon_oxide Ananth SmallScan CHRYSALIS_INC HighResolution AmplitudeModulation thermoplastic_elastomers Anneal HexacontaneFilm ScanningThermalMicroscopy Heating ULCA NeodymiumMagnets India PetruPoni_Institute Styrene Mechinical FastScan EFMAmplitude PS_LDPE Korea EvatecAG Potential Cobalt-dopedIronOxide Tin sulfide FM_SKPM LeakageCurrent Galfenol lift_mode ForceMapping
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Collagen film phase change by temp
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan