PvdfFilm Mosfet Switching IISCBangalore Mechanical Graphite PrCurve tip_bias_mode Polydimethylsiloxane plastics PS_PVAC Nickel Piezoresponse CancerCell mono_layer Anneal oxide_layer phase_change MoS2 BTO SingleLayer Polystyrene NUSNNI ElectroChemical semifluorinated_alkanes Al2O3 HBN AtomicLayer SurfaceOxidation solar_cell NtuEee Tungsten_disulfide LMF EvatecAG MfmAmplitude
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
F14H20
Semifluorinated alkanes on Si.
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256
- Scan Mode: AM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256