ElectroDeposition GaAs ElectroChemical semifluorinated_alkanes Wang Deposition Switching Terrace 2dMaterials SrTiO3 HighResolution BreastCancerCell IndiumTinOxide Piranha ImideMonomer self_healing Magnets C_AFM Photovoltaics frequency_modulation InsulatorFilm BoronNitride HfO2 TemperatureControllerStage SmallScan Copper Sphere SingleCrystal Dr.JurekSadowski mechanical property RedBloodCell non_contact lithography Temperature China
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Collagen fibrils
Scanning Conditions
- System : NX10
- Scan Mode: Tapping in Liquid
- Scan Rate : ALL 0.3Hz
- Scan Size : 10μm2, 4μm2
- Pixel Size : ALL 256×256
- Cantilever : PPP-FMR (k=2.8N/m, f=75kHz)