Ceramics Ni-FeAlloy norganic Inorganic_Compound LifeScience StrontiuTitanate Polymer PDMS CancerCell PANI LightEmission CompactDisk BismuthVanadate DentalProsthesis hard_disk_media TPU Techcomp Copper MultiLayerCeramicCapacitor HiVacuum PrCurve BiasMode WPlug CNT domain_switching semifluorinated alkane suspended_graphene Copolymer ScanningKelvinProbeMicroscopy HumanHair OrganicSemiconductor SrO ContactMode Piezoelectric temp_control
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Graphene on SiO2
Scanning Conditions
- System: NX20
- Scan Mode: PinPoint mechanical mode
- Cantilever: NSC36C
- Approach/Retract speed : 2ms/2ms
- Scan Size: 10μm×10μm, 5μm×5μm
- Pixel: 256 × 256
- Scan Mode: PinPoint mechanical mode
- Cantilever: NSC36C
- Approach/Retract speed : 2ms/2ms
- Scan Size: 10μm×10μm, 5μm×5μm
- Pixel: 256 × 256