Nanotechnology Piezoresponse Moire Hexacontane self-assembled_monolayer Polyethylene Croatia MultiferroicMaterials Multiferroic_materials Solar Ucl Neodymium Cell ContactModeDots Etch BiFeO3 LiNbO3 Non-ContactMode BaTiO3 Topography hard_disk PVAC Litho Calcium LFM Perovskite epitaxy suspended_graphene Holes CompactDisk 2d_materials Granada Boron GranadaUniv ThermalConductivity
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
SnS2 Flakes
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC240TS (k=2N/m, f=70kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.4Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC240TS (k=2N/m, f=70kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.4Hz
- Pixel Size: 256 × 256