sputter Conductive AFM FailureAnlaysis PANI Multiferroic_materials Heating SiliconCrystal bias_mode I-VSpectroscopy hard_disk_media Composition MfmPhase electrospinning Hexylthiophene Hafnia Ptfe CalciumHydroxide pinpoint mode molecular_self_assembly Hexacontane PpLdpe medical Croatia norganic Polarization OpticalModulator Resistance phase_change Collagen silicon_carbide PtfeMembrane Sadowski IndiumTinOxide EFMAmplitude NusEce
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ER 316L Stainless Steel
The ferrite MFM phase has a striped appearance due to its ferromagnetic behavior, while the paramagnetic austenite phase shows a uniform appearance.
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm