Praseodymium molecular_self_assembly SetpointMode hydrocarbon BismuthFerrite #Materials Dimethicone mfm_amplitude mechanical property BaTiO3 FuelCell Conductivity electrospinning Aluminium_Oxide Silver Defects Bacterium Sulfur strontiu_titanate Microchannel LogAmplifier Chemical_Vapor_Deposition CalciumHydroxyapatite Writing Holes Spincast HumanHair lithography silicon_carbide Polymer PhaseChange CopperFoil SICM CeNSE_IISc self-assembled_monolayer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PVDF Fibrous Membrane
PVDF fibrous membrane made by electrospinning.
Scanning Conditions
- System: NX10
- Scan Mode: Pinpoint PFM
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.05Hz
- Pixel Size: 256 × 256
- Scan Mode: Pinpoint PFM
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.05Hz
- Pixel Size: 256 × 256