KelvinProbeForceMicroscopy molecular_beam TPU Nanopattern INSPParis Graphene Polyaniline alkanes HfO2 ElectroDeposition Typhimurium MfmAmplitude University_of_Regensburg Gold KevlarFiber Wafer DNAProtein UTEM SKPM Tungsten_disulfide tip_bias_mode plastics ChemicalCompound Singapore Anneal hard_disk Spincast SiliconOxide polyvinyl acetate HBN LowDensityPolyethylene Oxidation MeltingPoint Gallium_Arsenide Piranha
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
F14H20
Semifluorinated alkanes on Si.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 05Hz, 1Hz
- Pixel Size: 1024 × 512, 512 x 256
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 05Hz, 1Hz
- Pixel Size: 1024 × 512, 512 x 256