Heating LightEmiting SiliconOxide SrO Oxide Aggregated_molecules YttriaStabilizedZirconia BariumTitanate SKPM FAFailureAnlaysis Varistor RedBloodCell CalciumHydroxyapatite CP-AFM SiWafer SicMosfet HardDiskMedia #Materials MultiLayerCeramicCapacitor multi_layer SiliconeOxide Biofilm Hexatriacontane Nanofiber GalliumPhosphide Cobalt Global_Comm Steps ScanningTunnelingMicroscopy Laser AnodizedAluminumOxide Friction lift_mode Cobalt-dopedIronOxide LiftHeight
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Margarines
Phase change of Margarine surface by temperature control
Scanning Conditions
- System: NX10
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256