Mechanical Insulator kelvin probe force microscopy Adhesion ForceVolume AlkaneFilm RedBloodCell 2d_materials Electronics DNA molecular_beam Molybdenum_disulfide MolecularSelfAssembly SicMosfet Polyvinylidene_fluoride AM_SKPM PS_LDPE SiliconCrystal InsulatorFilm Gold Phthalocyanine heterojunctions Chemical Vapor Deposition Lateral_Force_Microscopy TyphimuriumBiofilm Foil Mfm NUS single_layer PtfeFilter HiVacuum cannabis Magnetic Fendb Alloy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
GaN on Si epi film
Scanning Conditions
- System : NX20
- Scan Mode: Non-contact
- Scan Rate : All 2 Hz
- Scan Size : 5µm2, 5µm2
- Pixel Size : ALL 512×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)