Worcester_Polytechnic_Institute Piezoelectric Sic AtomicSteps BoronNitride Anneal Protein Oxidation Change MultiLayerCeramicCapacitor Sulfur Bio Chrome hard_disk_media GaAs MolybdenumDisulfide Barium_titanate Collagen Austenite kelvin probe force microscopy Defects flakes Heating Magnetic Force Microscopy LateralPFM LFM 2dMaterials Chromium Magnets CalciumHydroxyapatite semifluorinated_alkanes InLiquid Leakage Polyvinylidene Film
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer-Ceramic composite
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm
- Scan Rate: 0.4Hz
- Pixel: 512×256