Terrace silicon_carbide 2d_materials MagneticPhase Silicon Iron NusEce NtuEee STM Inorganic Nanotechnology Inorganic_Compound CuParticle Boron Pinpoint EPFL Adhesion thermoplastic_elastomers InorganicCompound LiquidCrystal MetalCompound CeramicCapacitor Beads SelfAssembly layers Typhimurium light_emitting dielectric_trench DeoxyribonucleicAcid Mechanical 2-vinylpyridine organic_polymer ContactModeDot Steps NUS
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ceramic Portland cement
Scanning Conditions
- System : NX10
- Scan Mode: Tapping
- Scan Rate : 1Hz
- Scan Size : 1μm×1μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)