Steps mechanical property Hole DLaTGS Solar AnodizedAluminumOxide SFAs temp_control VortexCore self-assembled_monolayer lift_mode Glass block_copolymer Fe_film PolyvinylideneFluoride IMT_Bucharest HBN Water aluminum_nitride Corrosion gallium_nitride ContactMode ForceDistanceSpectroscopy lithography Global_Comm Magnetic Ferrite UnivMaryland PrCurve LiIonBattery Fluoride LiNbO3 Calcium CeNSE_IISc MultiLayerCeramicCapacitor
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Live fibraoblast cell
Scanning Conditions
- System : NX12
- Scan Mode: SICM
- Scan Rate : 0.1 Hz
- Scan Size : 20μm×20μm
- Pixel Size : 64×64
- Cantilever : Nano pipette