Kevlar PetruPoni PS_PVAC Topography kelvin probe force microscopy ImideMonomer blended polymers LifeScience Butterfly gallium_nitride Tapping Nanotechnology Protein PinpointNanomechanicalMode Vortex HighAcpectRatio vertical_PFM Ceramics oxide_layer Array mono_layer PVA IndiumTinOxide Austenite CNT Organic Sphere Aluminum amplitude_modulation CompactDisk molecular_self_assembly ElectrostaticForceMicroscopy CeNSE_IISc I-VSpectroscopy pulsed_laser_deposition
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hydro gel
Scanning Conditions
- System: NX10
- Scan Mode: NCM, Liquid mode
- Cantilever: BL-AC40 (k=0.1N/m, f=110kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1Hz
- Pixel: 512×256