SmallScan Heating cannabinoid StrontiuTitanate LiquidCell Hafnia MagneticForceMicroscopy tip_bias_mode Alloy Conduct BariumTitanate Hexatriacontane ElectroDeposition piezoelectric force microscopy EFM ForceDistanceSpectroscopy fe_nd_b KelvinProbeForceMicroscopy small_scan epitaxy Polydimethylsiloxane Bacteria polymeric_arrays Beads SSRM AAO ImideMonomer Film CalciumHydroxide TungstenDeposition Stiffness Magnetostrictive Electrode Croatia I-VSpectroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer patterns on Si (1/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.2Hz
- Pixel: 512×256