Leakage PVAP3HT StrontiuTitanate ElectroDeposition AtomicLayer fluoroaalkane Polypropylene ElectrostaticForceMicroscopy Alloy LaAlO3 Display Hafnia C_AFM Filter Granada PolyStylene Iron Array thermal_conductivity Pipette Chrome BismuthVanadate EPFL Tin disulfide HfO2 Barium_titanate ReflexLens Water CalciumHydroxyapatite Metal-organicComplex Vinylpyridine HexagonalBoronNitride MoirePattern #Materials Lift
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG Moire
Scanning Conditions
- System: NX10
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128