molecule Composition SurfaceOxidation GaP Filter NUSNNI Platinum ElectrostaticForceMicroscopy Typhimurium layers electrospinning Co/Cr/Pt GalliumPhosphide NusEce ScanningSpreadingResistanceMicroscopy Array CompactDisk Piezoelectric SetpointMode CP-AFM LiftHeight NanoLithography semifluorinated_alkanes UTEM SKKU PVAC TemperatureControl SiWafer nanobar HACrystal PinpointNanomechanicalMode flakes PhaseTransition self_assembly ULCA
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Co coated surface
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.7Hz
- Pixel: 512×256
- Lift height: 30nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.7Hz
- Pixel: 512×256
- Lift height: 30nm