Chungnam_National_University Dimethicone ForceVolumeImage PetruPoni PtfeFilter Hydroxyapatite LateralPFM conductive Nickel Resistance pinpoint mode dielectric trench LateralForceMicroscopy mechanical_property silicon_oxide optoelectronics BiFeO3 thermal_conductivity Polyethylene Layer IndiumTinOxide Annealed MoirePattern Cobalt SiliconCrystal self-assembly PMNPT DomainSwitching Worcester_Polytechnic_Institute China Aggregated_molecules HBN Silver Pvdf Sio2
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Pattern in Microchannel
Patterns are used to reduce liquid flow speed in microchannel.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 5μm×5μm
- Scan Rate:1Hz, 0.5Hz
- Pixel: 512×256, 512×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 5μm×5μm
- Scan Rate:1Hz, 0.5Hz
- Pixel: 512×256, 512×256