PMNPT INSP ShenYang CrystalGrowing PolyvinylideneFluoride SiliconOxide tip_bias_mode cooling MultiLayerCeramicCapacitor Force-distance LiBattery ChemicalCompound thermoplastic_elastomers Trench Singapore Strontium Transparent HiVacuum SurfaceOxidation atomic_steps Sapphire ContactMode BismuthVanadate Solution plastic MeltingPoint molecular_self_assembly electrospinning TappingMode fe_nd_b pulsed_laser_deposition bias_mode Patterns Forevision Growth
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CrAu surface
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 256×256